Posted: 08/13/2014 at 10:14pm
That's interesting because I think the DHS balls definitely got better in the last few years compared to before.
Subject: Would adding a little resin to the Plastic ball
Posted: 08/13/2014 at 10:14pm
![]()
Sifting through the DHS patents for the 40mm celluloid balls, the formula has been changed at least once circa 2003 and then again circa 2009. The first time was a filler replacement from titanium dioxide to zinc oxide. The second time was the combined use of fillers and the addition of acetyl tributyl citrate as another solvent and alcohol-soluble nylon as another toughening agent. As you can see, that's gonna take some time. |
That's interesting because I think the DHS balls definitely got better in the last few years compared to before.